Investigations on correlation between grain size and stress rupture property of GH4169 alloy

Tytuł:
Investigations on correlation between grain size and stress rupture property of GH4169 alloy
Autorzy:
WEI Kang
ZHANG Yong
WANG Tao
LI Zhao
WAN Zhipeng
Temat:
gh4169
grain size
stress rupture property
grain orientation
plastic deformation
Motor vehicles. Aeronautics. Astronautics
TL1-4050
Źródło:
Journal of Aeronautical Materials, Vol 40, Iss 1, Pp 93-99 (2020)
Wydawca:
Journal of Aeronautical Materials, 2020.
Rok publikacji:
2020
Kolekcja:
LCC:Motor vehicles. Aeronautics. Astronautics
Typ dokumentu:
article
Opis pliku:
electronic resource
Język:
Chinese
ISSN:
1005-5053
Relacje:
https://doaj.org/toc/1005-5053
DOI:
10.11868/j.issn.1005-5053.2019.000076
Dostęp URL:
https://doaj.org/article/97b443ddc6004652849026e261bbb721  Link otwiera się w nowym oknie
Numer akcesji:
edsdoj.97b443ddc6004652849026e261bbb721
Czasopismo naukowe
Taking GH4169 alloy large-size bar as research object, combined with the manufacturing process of the bar, the stress rupture properties of the specimens with different grain sizes were analyzed by means of OM, FE-SEM, EBSD and TEM. The results show that under the high temperature and stress of the long-lasting test, various grain size samples exhibit different stress rupture properties and grain orientation evolution. When the grain size is small, some orientation of〈101〉obviously rotates to 〈001〉or 〈111〉orientation where deformation and fracture occur. Besides, the coordination of macroscopic deformation of fine grain is better. These promote the effective release of stress concentration and then better plasticity. But the diffusion creep caused by more grain boundaries in the fine grain sample is unfavorable to the high temperature strength and cracks are prone to nucleate and expand at the grain boundary adjacent to the hard orientation of 〈111〉, thus the rupture life is reduced. In addition, the deformation of the fine grain sample is larger, mainly concentrated at grain boundaries, and the number fraction of large angle misorientation is more, which is easy to crack and reduce the life.

Ta witryna wykorzystuje pliki cookies do przechowywania informacji na Twoim komputerze. Pliki cookies stosujemy w celu świadczenia usług na najwyższym poziomie, w tym w sposób dostosowany do indywidualnych potrzeb. Korzystanie z witryny bez zmiany ustawień dotyczących cookies oznacza, że będą one zamieszczane w Twoim komputerze. W każdym momencie możesz dokonać zmiany ustawień dotyczących cookies