Decreasing Bio-Degradation Rate of the Hydrothermal-Synthesizing Coated Mg Alloy via Pre-Solid-Solution Treatment.
Autorzy:
Song D; College of Mechanics and Materials, Hohai University, Nanjing 210098, China. .; Suqian Research Institute of Hohai University, Suqian 223800, China. . Li C; College of Mechanics and Materials, Hohai University, Nanjing 210098, China. . Zhang L; Department of Materials Science and Engineering, North Carolina State University, Raleigh, NC 27695, USA. . Ma X; Department of Materials Science and Engineering, North Carolina State University, Raleigh, NC 27695, USA. . Guo G; College of Mechanics and Materials, Hohai University, Nanjing 210098, China. Guo_. Zhang F; College of Mechanics and Materials, Hohai University, Nanjing 210098, China. .; Department of Materials Science and Engineering, Kyushu University, Fukuoka 819-0395, Japan. . Jiang J; College of Mechanics and Materials, Hohai University, Nanjing 210098, China. .; Suqian Research Institute of Hohai University, Suqian 223800, China. . Ma A; College of Mechanics and Materials, Hohai University, Nanjing 210098, China. aibin-ma@hhu.edu.cn.; Suqian Research Institute of Hohai University, Suqian 223800, China. aibin-ma@hhu.edu.cn.
Pokaż więcej
Źródło:
Materials (Basel, Switzerland) [Materials (Basel)] 2017 Jul 27; Vol. 10 (8). Date of Electronic Publication: 2017 Jul 27.
Ta witryna wykorzystuje pliki cookies do przechowywania informacji na Twoim komputerze. Pliki cookies stosujemy w celu świadczenia usług na najwyższym poziomie, w tym w sposób dostosowany do indywidualnych potrzeb. Korzystanie z witryny bez zmiany ustawień dotyczących cookies oznacza, że będą one zamieszczane w Twoim komputerze. W każdym momencie możesz dokonać zmiany ustawień dotyczących cookies